Skip to main content
Contact Person: Mr. Li Zong testermachine@aliyun.com
CE Certified · ISO Compliant · Export Worldwide · · Privacy Policy
WhatsApp +86 186 0104 2089 testermachine@aliyun.com QQ 871507446
Solutions / Application

Evaluation of Weld Joint reliability in Drill tube Based on Heat Input Variation in Bending and Microstructure examine

Standard: ASTM A106 Authors: Sebayang A., Tarigan E., Kamil I., Sutrisno J. Source: International Journal of Engineering, Science and Information Technology (20

Evaluation of Weld Joint reliability in Drill tube Based on Heat Input Variation in Bending and Microstructure examine
Standard: ASTM A106
Authors: Sebayang A., Tarigan E., Kamil I., Sutrisno J.
Source: International Journal of Engineering, Science and Information Technology (2026)
DOI: 10.52088/ijesty.v6i1.1795

Drill tubes are critical components in oil, gas, and geothermal drilling operations, serving as conduits for circulating drilling fluids from the surface to the borehole while simultaneously transmitting mechanical loads. Due to severe operating conditions, including elevated pressure, cyclic loading, and corrosive environments, the integrity of welded joints in drill tubes must be ensured through appropriate welding methods and quality evaluation. This study investigates the effects of heat input variations on the mechanical properties and microstructural characteristics of welded joints in ASTM A106 Grade B steel tubes produced using Shielded Metal Arc Welding (SMAW) and Gas Metal Arc Welding (GMAW). Welding was performed using a single V-groove butt joint configuration in the 1G position with a constant welding current of 140 A. SMAW welding employed E7018 electrodes, while GMAW utilized ER70S-6 filler wire with a shielding gas mixture of 70% argon and 30% CO?. Mechanical performance was evaluated through bending tests, including root and face bends, in accordance with applicable standards. In addition, microstructural analysis of the weld metal and Heat Affected Zone (HAZ) was conducted using optical microscopy after chemical etching to identify phase distribution and grain morphology. The bending test results revealed that SMAW-welded joints exhibited higher ultimate stress (?u) values than GMAW-welded joints. The highest ?u value of 1327.14 MPa was obtained from the SMAW face bend specimen, while the lowest value of 922.10 MPa was recorded for the GMAW root bend specimen. Furthermore, face-bend tests consistently yielded higher ?u values than root-bend tests for both welding methods, indicating superior mechanical resistance at the weld surface. Microstructural observ
⚡ Get Solution Quotation

Contact us for free consultation, quotation and technical support.

Inquiry Now
WhatsApp QQ Email
Tel / WhatsApp: +86 186 0104 2089
Email: testermachine@aliyun.com
CE Certified · ISO 9001

Summary

Drill pipe weld joint reliability is evaluated by correlating welding heat input with bending performance and microstructure, so that process windows can be qualified for downhole tubular service.

Frequently Asked Questions

How does heat input affect drill pipe weld joints?

Heat input changes cooling rate and weld microstructure, which in turn alters hardness, toughness and bending resistance of the joint and heat-affected zone.

Which tests qualify the weld joint?

Guided bend tests, metallographic microstructure examination, hardness mapping and, where required, fatigue or pressure cycling of the welded tube.

Last updated: September 24, 2026 · RTPLINE technical team · All applications

Products

Related Equipment

Contact Us

Send Us a Message

Our technical team will reply within 24 hours.

Prefer instant chat? WhatsApp +86 186 0104 2089 · QQ 871507446 · testermachine@aliyun.com
Certified quality
CE, ISO 9001:2015 & ISO 14001
Global delivery
Equipment exported to 140+ countries
Engineered to your standard
ISO / ASTM / API 15S, custom pressure range
Privacy-first enquiry
GDPR-ready, no data resale, reply within 24 h